Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kareline Oy PPMS5050 Natural Fiber Reinforced Polypropylene for injection molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Kareline Oy Ltd
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kareline Oy PPMS5050 Natural Fiber Reinforced Polypropylene for injection molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Natural fiber reinforced thermoplastic composite for injection molding. Fiber ECF bleached softwood pulp. Matrix plastic polypropylen.Information provided by Kareline Oy Ltd
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Melt Flow 5.17 g/10 min
5.17 g/10 min
ISO 1133, 200°C/10kg
Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.0 MPa
8270 psi
ISO 527-1
Elongation at Break 4.3 %
4.3 %
ISO 527-1
Flexural Modulus 4.20 GPa
609 ksi
ISO 178
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179
Processing Properties Metric English Comments
Mold Temperature 50.0 - 70.0 °C
122 - 158 °F
Drying Temperature 80.0 °C
176 °F
10 hour, dehumidifying dryer
100 °C
212 °F
4 hour, dehumidifying dryer