Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kennametal Stellite Stellite® 19

Category Metal , Nonferrous Metal , Cobalt Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Stellite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Stellite® 19.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Can be machined with carbide tipped tools, but when hardness exceeds Rc55 it is best to grind. Applications include cutting tools, bearing races, guide rolls, and nozzle discs. Excellent resistance to hot abrasion and adhesive wear, low coefficient of friction. Resistant to atmospheric oxidation and forms only a thin adherent scale at red heat. Resists attack from wet chlorine and acetic acid (boiling), excellent resistance to 10% boiling nitric, and 10% sulfuric acid at room temperature. Fair resistance to concentrated nitric boiling and 10% boiling sulfuric. Poor resistance to 77% sulfuric boiling and reducing acids. Data provided by the manufacturer, Deloro Stellite, Inc.Product of former Deloro Stellite Inc.
Physical Properties Metric English Comments
Density 8.36 g/cc
0.302 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 45 - 60
45 - 60
Tensile Strength, Ultimate 724 MPa
105000 psi
(Tensile Yield Strength near U.T.S.)
Elongation at Break <= 1.0 %
<= 1.0 %
Modulus of Elasticity 234 GPa
33900 ksi
Ultimate Compressive Strength 2137 MPa
309900 psi
Izod Impact Unnotched 4.75 J
3.50 ft-lb
Thermal Properties Metric English Comments
CTE, linear 12.8 µm/m-°C

@Temperature 20.0 - 100 °C
7.11 µin/in-°F

@Temperature 68.0 - 212 °F
13.7 µm/m-°C

@Temperature 20.0 - 300 °C
7.61 µin/in-°F

@Temperature 68.0 - 572 °F
14.2 µm/m-°C

@Temperature 20.0 - 500 °C
7.89 µin/in-°F

@Temperature 68.0 - 932 °F
14.2 µm/m-°C

@Temperature 20.0 - 600 °C
7.89 µin/in-°F

@Temperature 68.0 - 1110 °F
14.8 µm/m-°C

@Temperature 20.0 - 700 °C
8.22 µin/in-°F

@Temperature 68.0 - 1290 °F
15.1 µm/m-°C

@Temperature 20.0 - 800 °C
8.39 µin/in-°F

@Temperature 68.0 - 1470 °F
16.9 µm/m-°C

@Temperature 20.0 - 1000 °C
9.39 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 14.7 W/m-K
102 BTU-in/hr-ft²-°F
Melting Point 1239 - 1299 °C
2262 - 2370 °F
Solidus 1239 °C
2262 °F
Liquidus 1299 °C
2370 °F
Component Elements Properties Metric English Comments
Carbon, C 1.8 %
1.8 %
Chromium, Cr 31 %
31 %
Cobalt, Co 52.2 %
52.2 %
As remainder
Iron, Fe 2.5 %
2.5 %
Nickel, Ni 1.0 %
1.0 %
Silicon, Si 1.0 %
1.0 %
Tungsten, W 10.5 %
10.5 %