Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kennametal Stellite Stellite® 22 Cobalt Alloy

Category Metal , Nonferrous Metal , Cobalt Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Stellite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Stellite® 22 Cobalt Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Kennametal Stellite'sâ„¢ cobalt base alloys are available as cobalt rods, cobalt electrodes, cobalt wire and cobalt powder.Cobalt alloys are used primarily for wear applications and are particularly well-suited for hardfacing applications.Information provided by Kennametal Stelliteâ„¢
Mechanical Properties Metric English Comments
Hardness, Rockwell C 41 - 49
41 - 49
Component Elements Properties Metric English Comments
Carbon, C 0.30 %
0.30 %
Chromium, Cr 28 %
28 %
Cobalt, Co >= 52.7 %
>= 52.7 %
as balance
Iron, Fe <= 3.0 %
<= 3.0 %
Molybdenum, Mo 12 %
12 %
Nickel, Ni 1.5 %
1.5 %
Other <= 0.50 %
<= 0.50 %
Silicon, Si <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
Application Technique PTA & laser deposition