Material Notes:
Thermoplastic sheet for signageApplications: Sign applications, radomes, other applications where a weatherable color over a white substrate is desirableFeatures: Kydex 101 is more rigid than most other thermoplastics resulting in parts that will deform less when loaded. Offers unsurpassed resistance to breakage. The cap offers excellent weatherability for use in outdoor applications. Since the substrate is white, it eliminates the need for painting which is required with other thermoplastics and with metal.Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ASTM D785
Tensile Strength, Ultimate 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 160 %
160 %
Modulus of Elasticity 2.319 GPa
336.3 ksi
Flexural Yield Strength 64.0 MPa
9280 psi
ASTM D790
Izod Impact, Notched 9.53 J/cm

@Temperature 23.0 °C
17.9 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
annealed; ASTM D648
Flammability, UL94 V-0
V-0
V-0, 5V; UL Standard 94
Processing Properties Metric English Comments
Processing Temperature 162 - 200 °C
324 - 392 °F
Forming Temperature