| Category | Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded |
| Manufacturer | LG Chemical |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | LG Chemical LI968W Co-Extrusion ASA.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.010 | 0.010 | Extrusion Molding |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
| Melt Flow | 12 g/10 min @Load 10.0 kg, Temperature 220 °C |
12 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 104 | 104 | ASTM D785 |
| Tensile Strength, Yield | 49.0 MPa @Thickness 3.20 mm |
7110 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
| Elongation at Break | 25 % @Thickness 3.20 mm |
25 % @Thickness 0.126 in |
50mm/min; ASTM D638 |
| Elongation at Yield | >= 6.0 % @Thickness 3.20 mm |
>= 6.0 % @Thickness 0.126 in |
50mm/min; ASTM D638 |
| Tensile Modulus | 2.06 GPa @Thickness 3.20 mm |
299 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
| Flexural Yield Strength | 78.5 MPa @Thickness 3.20 mm |
11400 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
| Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
| Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
| 0.392 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 | |
| 1.37 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.57 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 | |
| 1.77 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.31 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.40 mm |
205 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 87.0 °C @Thickness 6.40 mm |
189 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| Vicat Softening Point | 95.0 °C @Load 5.00 kg |
203 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
| Flammability, UL94 | HB @Thickness >=1.60 mm |
HB @Thickness >=0.0630 in |
|
| HB @Thickness >=3.20 mm |
HB @Thickness >=0.126 in |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 1 | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
| Zone 2 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
| Zone 3 | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
| Zone 4 | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
| Adapter Temperature | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
| Die Temperature | 210 - 250 °C | 410 - 482 °F | Extrusion Molding |
| Melt Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
| Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Top |
| 70.0 - 90.0 °C | 158 - 194 °F | Middle | |
| 70.0 - 100 °C | 158 - 212 °F | Bottom | |
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Extrusion Molding |
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Extrusion Molding |