Material Notes:
Pearlbondâ„¢ 550 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.Application: Pearlbondâ„¢ 550 can be added to formulations of REACTIVE POLYURETHANE HOT-MELTS (HMPUR), in order to improve the crystallisation speed.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 2781
Viscosity 2.70e+6 cP

@Temperature 130 °C
2.70e+6 cP

@Temperature 266 °F
Melt; ISO 1133
Melt Flow 10 - 30 g/10 min

@Load 2.16 kg,
Temperature 170 °C
10 - 30 g/10 min

@Load 4.76 lb,
Temperature 338 °F
ISO 1133
Thermal Properties Metric English Comments
Melting Point 66.0 - 70.0 °C
151 - 158 °F
MQSA 70 A
Processing Properties Metric English Comments
Moisture Content <= 0.150 %
<= 0.150 %
MQSA 44
Descriptive Properties Value Comments
Crystallization Rate 10-14 minutes
MQSA 12 B
OH Value < 3 mg/KOH/g
MQSA 47 A
Thermoplasticity Very High
MQSA 68A