Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucas-Milhaupt BRAZE 450 Silver Based Cadmium Free Filler Metal

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name BRAZE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt BRAZE 450 Silver Based Cadmium Free Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Characteristics:Braze 450 is an intermediate temperature cadmium free silver brazing filler metal with sufficient melting range (145EF) to properly braze joints with the range of fits encountered in commercial tubing and fittings. It has a slight tendency to liquate (i.e. separate into high and low melting constituents) if heated slowly through its melting range. Applications:Braze 450 has found considerable application in pipe brazing in the ship construction industry and for such items as band instruments, brass lamps, aircraft engine oil coolers, plus other situations where a high strength, ductile joint is required. It is a good, general purpose, brazing filler metal for use where a cadmium free filler metal is specified. Specifications:Braze 450 conforms to the following specifications- AWS A5.8 BAg-5, ASME Boiler & Pressure Vessel Code Sec. II C, SFA-5.8 BAg-5 Information provided by Lucas-Milhaupt, Inc.
Physical Properties Metric English Comments
Density 9.11 g/cc
0.329 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 172 - 207 MPa
25000 - 30000 psi
Copper butt joint
276 - 345 MPa
40000 - 50000 psi
Brass butt joint
310 - 379 MPa
45000 - 55000 psi
Nickel-Silver butt joint
Elongation at Break 13 - 22 %
13 - 22 %
% in 2", Copper butt joint
14 - 28 %
14 - 28 %
% in 2", Nickel-Silver butt joint
20 - 36 %
20 - 36 %
% in 2", Brass butt joint
Thermal Properties Metric English Comments
Melting Point 662.8 - 743 °C
1225 - 1370 °F
Solidus 662.8 °C
1225 °F
Melting Point
Liquidus 743 °C
1370 °F
Flow Point
Component Elements Properties Metric English Comments
Copper, Cu 29 - 31 %
29 - 31 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 44 - 46 %
44 - 46 %
Zinc, Zn 23 - 27 %
23 - 27 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000908 ohm-cm
0.00000908 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 743 - 843 °C
1370 - 1550 °F
Brazing Range
Descriptive Properties Value Comments