Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucas-Milhaupt Silvaloy® A45T Brazing Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name Silvaloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Silvaloy® A45T Brazing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Silvaloy A45T is a free flowing, low melting and an excellent substitute to the cadmium bearing filler metals with similar silver contents. Silvaloy A45T narrow melt range makes it suitable for manual or machine feeding into the braze joint. The alloy is best suited for narrow gap filling in the range of 0.001 - 0.005 inches. Typical applications are the joining of ferrous, non-ferrous, and dissimilar metals and alloys with close joint clearances.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 8.95 g/cc
8.95 g/cc
Density 8.96 g/cc
0.324 lb/in³
Thermal Properties Metric English Comments
Melting Point 646.1 - 688 °C
1195 - 1270 °F
Solidus 646.1 °C
1195 °F
Liquidus 688 °C
1270 °F
Maximum Service Temperature, Air 204 °C
400 °F
continuous
316 °C
600 °F
intermittent
Component Elements Properties Metric English Comments
Copper, Cu 26 - 28 %
26 - 28 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 44 - 46 %
44 - 46 %
Tin, Sn 2.5 - 3.5 %
2.5 - 3.5 %
Zinc, Zn 23 - 27 %
23 - 27 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000960 ohm-cm
0.00000960 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 710 - 843 °C
1310 - 1550 °F
Brazing Temperature
Descriptive Properties Value Comments
Color Pale Yellow
Electrical Conductivity (% IACS) 18
Users viewing this material also viewed the following: