LyondellBasell Hostacomâ„¢ BG751P Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Manufacturer LyondellBasell
Trade Name Hostacom™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hostacomâ„¢ BG751P Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Hostacomâ„¢ BG751P very high melt flow, 1,600 MPa flexural modulus, UV-stabilized, natural, 20% calcium carbonate-filled, modified polypropylene resin has a unique balance of processability and weatherability. It was designed for applications that undergo extended outdoor exposure. Features include: superior moldfilling capability, excellent weatherability, good impact/stiffness balance, and excellent surface appearance. Typical applications include residential siding panels. Uses: Outdoor applicationsInformation provided by Basell.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ISO 1183
Melt Flow 70 g/10 min

@Load 2.16 kg,
Temperature 230 °C
70 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa
3190 psi
ISO 527-1, -2
Elongation at Break 30 %
30 %
ISO 527-1, -2
Flexural Modulus 1.60 GPa
232 ksi
ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature -30.0 - 100 °C
44.4 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM D696