Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M Chemical GUARD DOGâ„¢ UV622 HALS Light Stabilizer

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer M Chemical Company, Inc.
Trade Name GUARD DOG™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M Chemical GUARD DOGâ„¢ UV622 HALS Light Stabilizer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
GUARD DOG™ UV662 is a solid, polymeric type, free radical scavenger hindered amine light stabilizer that is used to protect a wide range of polymers against degradation caused by exposure to UV radiation. It is used in applications that demand low volatility and minimal surface migration.It provides light stability to thick and thin sections and contributes significantly to the long term heat stability of polyolefins and tackifier resins, It has a low melting range and has excellent thermal stability. It is compatible with a wide range of resin systems and is un-extractable in aqueous conditions. This product typically demonstrates reduced interaction with co-additives such as pigments or other stabilizers and can easily be dispersed.GUARD DOG™ UV662 shows strong synergistic performance when used in combination with other GUARD DOG™ UV Absorber, HALS and Antioxidant products.Applications: GUARD DOG™ UV662 is extremely effective in PE, PP, SAN, ASA, SBS, PS, polyurethanes, polyamides, unsaturated polyesters, and polyacetals including plastisols, elastomers, adhesives, sealants and films.Typical Properties: 67, Xylene - 8TGA analysis (10 mg@10°C/min) under nitrogen atmosphere shows = 1% weight loss at 250°C, = 3% at 300°C and = 8.5% at 325°C.volatile loss at 105°C for 2 hours = 0.5%
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc

@Temperature 35.0 °C
1.22 g/cc

@Temperature 95.0 °F
Bulk Density 0.570 g/cc
0.0206 lb/in³
Molecular Weight >= 2000 g/mol
>= 2000 g/mol
Ash <= 0.10 %
<= 0.10 %
Thermal Properties Metric English Comments
Softening Point 55.0 - 85.0 °C
131 - 185 °F
Flash Point >= 250 °C
>= 482 °F
Optical Properties Metric English Comments
UV Transmittance >= 97 %

@Thickness 0.425 mm
>= 97 %

@Thickness 0.0167 in
10g/100ml of Methyl Benzene
>= 99 %

@Thickness 0.500 mm
>= 99 %

@Thickness 0.0197 in
10g/100ml of Methyl Benzene
Component Elements Properties Metric English Comments
Nitrogen, N 4.9 %
4.9 %
Descriptive Properties Value Comments
CAS Number 65447-77-0
Molecular Formula C28H52O4N2
Name Poly-(N-beta-hydroxyethyl-2,2,6,6-tetramethyl-4-hydroxy-piperidyl-succinate)
Recommended Dosage 0.10 - 1.20%
depending upon the substrate and performance requirements