Material Notes:
Corrosion resistance and high strength. Produced under license of ARMCO Advanced Materials Corp. Applications: Deck equipment, pumps, valves.Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 179
179
Tensile Strength, Ultimate >= 585 MPa
>= 84800 psi
Tensile Strength, Yield >= 290 MPa
>= 42100 psi
Elongation at Break >= 30 %
>= 30 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.060 %
<= 0.060 %
Chromium, Cr 20.5 - 23.5 %
20.5 - 23.5 %
Iron, Fe 51.94 - 62.1 %
51.94 - 62.1 %
As Balance
Manganese, Mn 4.0 - 6.0 %
4.0 - 6.0 %
Molybdenum, Mo 1.5 - 3.0 %
1.5 - 3.0 %
Nickel, Ni 11.5 - 13.5 %
11.5 - 13.5 %
Niobium, Nb (Columbium, Cb) 0.10 - 0.30 %
0.10 - 0.30 %
Nitrogen, N 0.20 - 0.40 %
0.20 - 0.40 %
Silicon, Si <= 1.0 %
<= 1.0 %
Vanadium, V 0.10 - 0.30 %
0.10 - 0.30 %
Descriptive Properties Value Comments
Heat Treatment Sol. Anneal