| Category | Ceramic , Oxide , Aluminum Oxide |
| Manufacturer | Misumi |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Misumi Alumina 96 Aluminum Oxide, Al2O3.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.70 g/cc | 0.134 lb/in³ | |
| Water Absorption | 0.000 % | 0.000 % |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 300 MPa | 43500 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 500 °C |
4.06 µin/in-°F @Temperature 68.0 - 932 °F |
|
| 8.00 µm/m-°C @Temperature 20.0 - 800 °C |
4.44 µin/in-°F @Temperature 68.0 - 1470 °F |
||
| Thermal Conductivity | 18.0 W/m-K | 125 BTU-in/hr-ft²-°F | |
| Melting Point | 2050 °C | 3720 °F | |
| Maximum Service Temperature, Air | 1300 °C | 2370 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 96.0 % | 96.0 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | |
| Dielectric Constant | 9.00 | 9.00 | |
| Dielectric Strength | >= 10.0 kV/mm | >= 254 kV/in | |
| Dielectric Loss Index | 0.000100 | 0.000100 |