Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials RTV162 Electronic Grade Silicone Adhesive Sealant, White

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials RTV162 Electronic Grade Silicone Adhesive Sealant, White.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature. These electronic grade silicone adhesive sealants differ somewhat in physical properties including consistency.Key Performance Properties: Non-corrosive to electronic metals, including copper and brassLow odor cure, releasing an alcohol vapor from the sealant surface during cureUL recognitionRetains elastomeric properties for long periods at temperatures from 60°C to 205°C and for short periods up to 260°COne-componentCure at room temperatureExcellent electrical insulation propertiesExcellent resistance to moisture, dust, dirt, UV, ozone, and chemicalsGE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
Tensile Strength, Ultimate 3.75 MPa
543 psi
Elongation at Break 400 %
400 %
Peel Strength 7.01 kN/m
40.0 pli
1 in. x 8in. Stainless steel screen at 180° pull angle
Thermal Properties Metric English Comments
CTE, linear 270 µm/m-°C

@Temperature 20.0 °C
150 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
399 °F
Continuous
260 °C
500 °F
Intermittent
Brittleness Temperature -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+15 ohm-cm
3.00e+15 ohm-cm
Dielectric Constant 2.8

@Frequency 60 Hz
2.8

@Frequency 60 Hz
Dielectric Strength 18.0 kV/mm
457 kV/in
Dissipation Factor 0.0010

@Frequency 60 Hz
0.0010

@Frequency 60 Hz
Processing Properties Metric English Comments
Cure Time 200 min
4 hour
Tack-free
Descriptive Properties Value Comments
Application rate 350 g/min
Color White
Consistency Spreadable paste