Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 18.0 kV/mm | 457 kV/in | IEC 60243-1 |
Murtfeldt Murinyl® Polyvinylidinefluoride As a fluorinated plastic, Murinyl® is exceptionally resistant to chemicals, hydrolysis, and sterilization. Its properties change very little at high service temperatures and after long-term exposur.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 6 BT Polyamide 6 FeaturesBasic type PA 6 for injection moulding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical .. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Premix Premi-Glas® 3101-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-10 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 6 BT LS Polyamide 6, UV Stabilized FeaturesPA 6 for injection moulding with the content of UV stabilizer predetermines products for external use, eg. seats for sport stadiums, covers of electrical appliances. Delivered in natural an.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.00 mm |
457 kV/in @Thickness 0.118 in |
ASTM D149 |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra.. |
|||
Dielectric Strength | 18.0 - 50.0 kV/mm | 457 - 1270 kV/in | Average value: 33.2 kV/mm Grade Count:16 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | |
Cookson Group Plaskon® 3200LS Mineral Filled Novolac Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability under very stringent testing. This material is designed to minimize stress on the encapsulated .. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | AC 60 Hz |
Fujipoly Industries Sarcon® 45GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | 60°C for 1,000 hrs with 90% RH; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-Hn Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | Perpendicular, Short-term, in air; ASTM D149 |
Glastic Laminates/Shapes FHT Flexible High Temperature Polyester Laminate Data provided by Glastic Corporation.Excellent flexibility plus good electrical strength retention values after long term heat aging. Widely used in motors and dry type transformers. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® R-7-190BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 9076 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East) NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | IEC 60250 |
Polyram RamLloy PN300G2 PPE/PS Alloy, 10% Glass Fiber PPE/PS alloy, 10% glass fiber reinforced for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | IEC 60250 |
Polyram RamLloy PN300G6 PPE/PS Alloy, 30% Glass Fiber PPE/PS alloy, 30% glass fiber reinforced for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | IEC 60243-1 |
Polyplastics Duracon® SF-20 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | IEC 60243-1 |
Polyplastics Duracon® SW-01 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 411 Paper, 5 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | AC Rapid Rise; ASTM D149 |
DuPont™ Nomex® E56 Paper, 12 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | AC Rapid Rise; ASTM D149 |
DuPont™ Nomex® E56 Paper, 7 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | Insulating Strength |
China-Yixing Longly Refractories Zirconia Ceramics LONGLY provides a multitude of zirconia products including balls, plates, tubes, rods and etc. by adopting magnesia, calcia or yttria stabilized zirconia powder as raw material through dry pressing,.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Ashley Polymers Ashlene® 527LD Nylon 66 A very high impact, slightly lubricated nylon resin.Data provided by the manufacturer |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Ashley Polymers Ashlene® 527LDS Nylon 66 A very high impact, slightly lubricated and heat stabilized nylon resin.Data provided by the manufacturer |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | in transformer oil; IEC 60243-1 |
CENTROPLAST CENTROPHEN GF Polyphenylene ether 30% glass fiber This material is a lightweight plastic with low moisture absorption, and is impact resistant at low temperatures. Applications include electronic housings, valve pistons, and support rollers.Inform.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 2.00 mm |
457 kV/in @Thickness 0.0787 in |
IEC 243-1 |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® BR111 is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical .. |