Momentive Performance Materials Silpruf® Construction Sealant

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Construction Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name Silpruf®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials Silpruf® Construction Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
One-part, for weatherseals, structural glazing, and general purpose sealing. Cure Method: Alkoxy (Neutral). Tack-free time 5 to 10 hr.; Peel Strength 55 lb/in.; Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
ASTM D2240
Tensile Strength, Ultimate 2.00 MPa
290 psi
ASTM D412
Tensile Strength, Yield 0.240 MPa
34.8 psi
at 50% Extension (0.5 x 0.38 x 2 in bead)
Tear Strength 3.50 kN/m
20.0 pli
ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Elasticity is retained to this temperature.
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
Elasticity is retained to this temperature.
Processing Properties Metric English Comments
Processing Temperature 27.0 °C
80.6 °F
Cure time to 0.38 in. is 10-14 days