Multibase Multi-Flex® TPO A-7507

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO A-7507.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TPO compound suitable for carpet backing seals.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792-91
Melt Flow 1.5 g/10 min
1.5 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 5.00 MPa
725 psi
ASTM D638-95
Elongation at Break 300 %
300 %
ASTM D638-95
Flexural Modulus 0.0669 GPa
9.70 ksi
Method 1, Proc. B; ASTM D-790-95
Tear Strength 35.0 kN/m
200 pli
ASTM D624-95