Multibase Multi-Pro® 2012 RC 20% Glass Filled Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Multibase
Trade Name Multi-Pro®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 2012 RC 20% Glass Filled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Moisture content is 0.06%. Multi-Pro 2012 RC is a glass reinforced polypropylene, chemically coupled which enhances the mechanical properties. This product has been formulated to achieve an esthetic surface.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792-91
Melt Flow 8.0 g/10 min
8.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 48.3 MPa
7010 psi
ASTM D638-95
Elongation at Break 18 %
18 %
ASTM D638-95
Flexural Strength 69.0 MPa
10000 psi
ASTM D790-92
Flexural Modulus 3.103 GPa
450.1 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256-93a
Gardner Impact 0.300 J
0.221 ft-lb
ASTM D5420-93