Material Notes:
NYCOA 534 H is a high viscosity; heat stabilized, nucleated Nylon 6 resin. The high viscosity and fast set-up time make an excellent material for extrusion of tubing, rods, sheet and film. Because of its fast set-up time, fast extrusion line speeds have been achieved. NYCOA 534 H is suitable for applications that require continuous exposure to temperatures in excess of 110° C.Information provided by Nycoa, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Water Absorption 1.8 %
1.8 %
24 hours; ASTM D570
Viscosity Measurement 4.0 - 4.4
4.0 - 4.4
Relative, Sulfuric Acid; NYCOA test
145 - 200
145 - 200
Relative, Formic Acid; NYCOA test
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Yield 83.0 MPa
12000 psi
ASTM D638
Elongation at Break 130 %
130 %
ASTM D638
Flexural Strength 114 MPa
16500 psi
ASTM D790
Flexural Modulus 2.689 GPa
390.0 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 191 °C
376 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C
151 °F
ASTM D648
Descriptive Properties Value Comments
Water Extractables, % 0.8