Material Notes:
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 0.886 g/cc
0.886 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.010 cm/cm

@Thickness 3.17 mm
0.010 in/in

@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0090 cm/cm

@Thickness 3.17 mm
0.0090 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 0.70 g/10 min

@Load 1.00 kg,
Temperature 235 °C
0.70 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
4.6 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.6 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 68
58 - 68
10 second dwell; ASTM D2240
61 - 71
61 - 71
Instantaneous; ASTM D2240
Tensile Strength, Yield 12.1 MPa
1750 psi
chs 20 in/min; ASTM D412
Elongation at Break 720 %
720 %
ASTM D412
Flexural Modulus 0.0185 GPa
2.69 ksi
ASTM D790
Tear Strength 35.0 kN/m
200 pli
ASTM D624