| Category | Fluid , Lubricant , Perfluoropolyether (PFPE) , PTFE Gellant |
| Manufacturer | Nye Lubricants |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Nye Lubricants 833Z-1 (FG) Synthetic Oil.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity Measurement | 90 | 90 | Viscosity Index of Base Oil; ASTM D2270 |
| Kinematic Viscosity at 40°C (104°F) | 23 cSt | 23 cSt | Base Oil; ASTM D445 |
| Kinematic Viscosity at 100°C (212°F) | 4.0 cSt | 4.0 cSt | Base Oil; ASTM D445 |
| Evaporation Loss | 5.0 % | 5.0 % | 24 hrs, 100C; ASTM D972 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Penetration P(0), 1/10 mm | 350 | 350 | ASTM D217 |
| Penetration P(60), 1/10 mm | 410 | 410 | ASTM D217 |
| Oil Separation | 15 % | 15 % | 24 hrs, 100C; FTM 719B, 321.2 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 175 °C | 347 °F | Recommended |
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Recommended |
| Pour Point | -63.0 °C | -81.4 °F | Base Oil; ASTM D97 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Base Fluid Type | PFPE(pnd) | |
| Gellant Type | PTFE |