| Category | Fluid , Lubricant , Perfluoropolyether (PFPE) , PTFE Gellant |
| Manufacturer | Nye Lubricants |
| Trade Name | UniFlor |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Nye Lubricants UniFlor 8612 (849) (UF) Synthetic Oil.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity Measurement | 126 | 126 | Viscosity Index of Base Oil; ASTM D2270 |
| Kinematic Viscosity at 40°C (104°F) | 345 cSt | 345 cSt | Base Oil; ASTM D445 |
| Kinematic Viscosity at 100°C (212°F) | 33 cSt | 33 cSt | Base Oil; ASTM D445 |
| Evaporation Loss | 0.30 % | 0.30 % | 22 hrs, 150C; ASTM D972 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Penetration P(0), 1/10 mm | 230 | 230 | ASTM D217 |
| Penetration P(60), 1/10 mm | 239 | 239 | ASTM D217 |
| Oil Separation | 3.0 % | 3.0 % | 22 hrs, 150C; FTM 719B, 321.2 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 250 °C | 482 °F | Recommended |
| Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | Recommended |
| Pour Point | -25.0 °C | -13.0 °F | Base Oil; ASTM D97 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Base Fluid Type | PFPE(pnd) | |
| Gellant Type | PTFE |