Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® 600 Nylon 6, 50% RH, Extrusion Grade

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer Nylene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® 600 Nylon 6, 50% RH, Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Extrusion grade. Nylene 600 is a general purpose, medium viscosity, extrusion grade resin used in applications such as rods, slabs, and tubing. Other applications include wire jacketing and centrifugal casting which require good dielectric properties, toughness, and fatigue resistance. Optimum processing conditions should provide a melt temperature of 480 - 500ºF at the die.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Yield Strength 28.0 MPa
4060 psi
ASTM D790
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 255 °C
491 °F