Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Construction Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.37 - 1.52 g/cc
0.0495 - 0.0549 lb/in³
Average value: 1.47 g/cc Grade Count:6
Mechanical Properties Metric English Comments
Hardness, Shore A 18.0 - 40.0
18.0 - 40.0
Average value: 32.6 Grade Count:14
Tensile Strength, Ultimate 1.20 - 5.50 MPa
174 - 798 psi
Average value: 2.39 MPa Grade Count:14
Tensile Strength, Yield 0.240 - 0.590 MPa
34.8 - 85.6 psi
Average value: 0.339 MPa Grade Count:7
Elongation at Break 200 - 500 %
200 - 500 %
Average value: 371 % Grade Count:7
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 88.0 - 204 °C
190 - 399 °F
Average value: 136 °C Grade Count:10
Minimum Service Temperature, Air -62.0 - -48.0 °C
-79.6 - -54.4 °F
Average value: -57.3 °C Grade Count:9
Processing Properties Metric English Comments
Processing Temperature 25.0 - 27.0 °C
77.0 - 80.6 °F
Average value: 26.2 °C Grade Count:13