Parker Chomerics CHO-MUTE 9025 Conductive Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-MUTE
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Parker Chomerics CHO-MUTE 9025 Conductive Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicone polymer system that offers the benefit of wide band absorption and high permeability in a lightweight and flexible product form.Typical Applications: Hand held electronics; Wireless voice or data telecommunication; Military electronics; GPS; Ruggedized computers; Night vision and Telecommunication infrastructure equipment.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 3.40 g/cc
3.40 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
ASTM D2240
Tensile Strength 3.44 MPa
499 psi
ASTM D412
Elongation at Break >= 200 %
>= 200 %
ASTM D412
Tear Strength 10.5 kN/m
60.0 pli
ASTM D624
Thermal Properties Metric English Comments
Thermal Conductivity 0.870 W/m-K
6.04 BTU-in/hr-ft²-°F
ASTM D5470
Maximum Service Temperature, Air 160 °C
320 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm
Bulk, Initial; CEPS-0002
Surface Resistivity per Square >= 1.00e+6 ohm
>= 1.00e+6 ohm
Initial; CEPS-0002
Magnetic Permeability 1.76
1.76
ASTM D2520
Shielding Effectiveness -20.0 dB
<br>@Thickness 2.36 mm,<br> Frequency 6.00e+9 Hz
-20.0 dB
<br>@Thickness 0.0930 in,<br> Frequency 6.00e+9 Hz
Microwave Absorption
-15.0 dB
<br>@Thickness 1.57 mm,<br> Frequency 9.80e+9 Hz
-15.0 dB
<br>@Thickness 0.0620 in,<br> Frequency 9.80e+9 Hz
Microwave Absorption
-13.0 dB
<br>@Thickness 0.813 mm,<br> Frequency 1.08e+10 Hz
-13.0 dB
<br>@Thickness 0.0320 in,<br> Frequency 1.08e+10 Hz
Microwave Absorption
-12.0 dB
<br>@Thickness 1.57 mm,<br> Frequency 1.08e+10 Hz
-12.0 dB
<br>@Thickness 0.0620 in,<br> Frequency 1.08e+10 Hz
Microwave Absorption
-11.0 dB
<br>@Thickness 0.813 mm,<br> Frequency 1.28e+10 Hz
-11.0 dB
<br>@Thickness 0.0320 in,<br> Frequency 1.28e+10 Hz
Microwave Absorption
-11.0 dB
<br>@Thickness 15.7 mm,<br> Frequency 8.80e+9 Hz
-11.0 dB
<br>@Thickness 0.620 in,<br> Frequency 8.80e+9 Hz
Microwave Absorption
-10.0 dB
<br>@Thickness 2.36 mm,<br> Frequency 8.80e+9 Hz
-10.0 dB
<br>@Thickness 0.0930 in,<br> Frequency 8.80e+9 Hz
Microwave Absorption
-10.0 dB
<br>@Thickness 3.17 mm,<br> Frequency 2.80e+9 Hz
-10.0 dB
<br>@Thickness 0.125 in,<br> Frequency 2.80e+9 Hz
Microwave Absorption
-10.0 dB
<br>@Thickness 0.813 mm,<br> Frequency 8.80e+9 Hz
-10.0 dB
<br>@Thickness 0.0320 in,<br> Frequency 8.80e+9 Hz
Microwave Absorption
-7.00 dB
<br>@Thickness 1.57 mm,<br> Frequency 6.80e+9 Hz
-7.00 dB
<br>@Thickness 0.0620 in,<br> Frequency 6.80e+9 Hz
Microwave Absorption
-7.00 dB
<br>@Thickness 3.17 mm,<br> Frequency 4.80e+9 Hz
-7.00 dB
<br>@Thickness 0.125 in,<br> Frequency 4.80e+9 Hz
Microwave Absorption
-6.00 dB
<br>@Thickness 3.17 mm,<br> Frequency 6.80e+9 Hz
-6.00 dB
<br>@Thickness 0.125 in,<br> Frequency 6.80e+9 Hz
Microwave Absorption
-6.00 dB
<br>@Thickness 2.36 mm,<br> Frequency 1.08e+10 Hz
-6.00 dB
<br>@Thickness 0.0930 in,<br> Frequency 1.08e+10 Hz
Microwave Absorption
-6.00 dB
<br>@Thickness 0.813 mm,<br> Frequency 6.80e+9 Hz
-6.00 dB
<br>@Thickness 0.0320 in,<br> Frequency 6.80e+9 Hz
Microwave Absorption
-5.00 dB
<br>@Thickness 0.508 mm,<br> Frequency 1.08e+10 Hz
-5.00 dB
<br>@Thickness 0.0200 in,<br> Frequency 1.08e+10 Hz
Microwave Absorption
-4.00 dB
<br>@Thickness 1.57 mm,<br> Frequency 2.80e+9 Hz
-4.00 dB
<br>@Thickness 0.0620 in,<br> Frequency 2.80e+9 Hz
Microwave Absorption
-3.00 dB
<br>@Thickness 2.36 mm,<br> Frequency 2.80e+9 Hz
-3.00 dB
<br>@Thickness 0.0930 in,<br> Frequency 2.80e+9 Hz
Microwave Absorption
-3.00 dB
<br>@Thickness 0.508 mm,<br> Frequency 6.80e+9 Hz
-3.00 dB
<br>@Thickness 0.0200 in,<br> Frequency 6.80e+9 Hz
Microwave Absorption
-3.00 dB
<br>@Thickness 3.17 mm,<br> Frequency 8.80e+9 Hz
-3.00 dB
<br>@Thickness 0.125 in,<br> Frequency 8.80e+9 Hz
Microwave Absorption
-3.00 dB
<br>@Thickness 0.254 mm,<br> Frequency 1.08e+10 Hz
-3.00 dB
<br>@Thickness 0.0100 in,<br> Frequency 1.08e+10 Hz
Microwave Absorption
-3.00 dB
<br>@Thickness 0.813 mm,<br> Frequency 2.80e+9 Hz
-3.00 dB
<br>@Thickness 0.0320 in,<br> Frequency 2.80e+9 Hz
Microwave Absorption
-2.00 dB
<br>@Thickness 0.254 mm,<br> Frequency 6.80e+9 Hz
-2.00 dB
<br>@Thickness 0.0100 in,<br> Frequency 6.80e+9 Hz
Microwave Absorption
-2.00 dB
<br>@Thickness 3.17 mm,<br> Frequency 1.08e+10 Hz
-2.00 dB
<br>@Thickness 0.125 in,<br> Frequency 1.08e+10 Hz
Microwave Absorption
-1.00 dB
<br>@Thickness 0.508 mm,<br> Frequency 2.80e+9 Hz
-1.00 dB
<br>@Thickness 0.0200 in,<br> Frequency 2.80e+9 Hz
Microwave Absorption
-1.00 dB
<br>@Thickness 0.254 mm,<br> Frequency 2.80e+9 Hz
-1.00 dB
<br>@Thickness 0.0100 in,<br> Frequency 2.80e+9 Hz
Microwave Absorption
0.00 dB
<br>@Thickness 0.508 mm,<br> Frequency 8.00e+8 Hz
0.00 dB
<br>@Thickness 0.0200 in,<br> Frequency 8.00e+8 Hz
Microwave Absorption
0.00 dB
<br>@Thickness 3.17 mm,<br> Frequency 8.00e+8 Hz
0.00 dB
<br>@Thickness 0.125 in,<br> Frequency 8.00e+8 Hz
Microwave Absorption
0.00 dB
<br>@Thickness 0.254 mm,<br> Frequency 8.00e+8 Hz
0.00 dB
<br>@Thickness 0.0100 in,<br> Frequency 8.00e+8 Hz
Microwave Absorption
0.00 dB
<br>@Thickness 2.36 mm,<br> Frequency 8.00e+8 Hz
0.00 dB
<br>@Thickness 0.0930 in,<br> Frequency 8.00e+8 Hz
Microwave Absorption
0.00 dB
<br>@Thickness 0.813 mm,<br> Frequency 8.00e+8 Hz
0.00 dB
<br>@Thickness 0.0320 in,<br> Frequency 8.00e+8 Hz
Microwave Absorption
0.00 dB
<br>@Thickness 1.57 mm,<br> Frequency 8.00e+8 Hz
0.00 dB
<br>@Thickness 0.0620 in,<br> Frequency 8.00e+8 Hz
Microwave Absorption
Dielectric Constant 13.8
13.8
ASTM D2520
Dielectric Loss Index 0.15
0.15
ASTM D2520
Descriptive Properties Value Comments
Composition Ferrous filled silicone
Magnetic Loss Tangent 0.602
ASTM D2520