| Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone |
| Manufacturer | Parker Chomerics |
| Trade Name | CHO-SEAL |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Parker Chomerics CHO-SEAL 1485 Conductive Elastomer.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.45 - 1.95 g/cc | 1.45 - 1.95 g/cc |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 55 - 65 | 55 - 65 | |
| Tensile Strength at Break | >= 1.24 MPa | >= 180 psi | ASTM D412 |
| Elongation at Break | >= 100 % | >= 100 % | ASTM D412 |
| Tear Strength | 5.25 kN/m | 30.0 pli | |
| Compression Set | 30 % | 30 % | 70 hrs @ 100°C; ASTM D395 Method B |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
| Minimum Service Temperature, Air | -40.0 °C | -40.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 0.020 ohm-cm | 0.020 ohm-cm | as supplied without pressure sensitive adhesive |
| Shielding Effectiveness | >= 50 dB | >= 50 dB | 200 kHz (H Field); MIL-G-83528 |
| >= 80 dB | >= 80 dB | 10 GHz (Plane Wave); MIL-G-83528 | |
| >= 90 dB | >= 90 dB | 2 GHz (Plane Wave); MIL-G-83528 | |
| >= 100 dB | >= 100 dB | 100 MHz (E Field); MIL-G-83528 | |
| >= 100 dB | >= 100 dB | 500 MHz (E Field); MIL-G-83528 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Binder | Silicone | |
| EMP Survivability kA / in, min | 0.3 | |
| Filler | Ag/Al | |
| Heat Aging ohm-cm max | 0.06 | |
| Vibration Resistance, After, ohm-cm max | 0.02 | |
| Vibration Resistance, During, ohm-cm max | 0.06 |