| Category | Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI) + PCE |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | ULTEM |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.47 g/cc | 1.47 g/cc | ASTM D 792 |
| Density | 1.47 g/cc | 0.0531 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 0.20 % | 0.20 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.50 % @Temperature 23.0 °C |
0.50 % @Temperature 73.4 °F |
ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on tensile bar; SABIC Method |
| 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method | |
| Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 360 °C |
28 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| 30 g/10 min @Load 6.60 kg, Temperature 337 °C |
30 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 143 MPa | 20700 psi | 5 mm/min; ISO 527 |
| 144 MPa | 20900 psi | Type I, 5 mm/min; ASTM D 638 | |
| Tensile Strength, Yield | 143 MPa | 20700 psi | 5 mm/min; ISO 527 |
| 144 MPa | 20900 psi | Type I, 5 mm/min; ASTM D 638 | |
| Elongation at Break | 2.4 % | 2.4 % | 5 mm/min; ISO 527 |
| 2.5 % | 2.5 % | Type I, 5 mm/min; ASTM D 638 | |
| Elongation at Yield | 2.4 % | 2.4 % | 5 mm/min; ISO 527 |
| 2.5 % | 2.5 % | Type I, 5 mm/min; ASTM D 638 | |
| Tensile Modulus | 9.68 GPa | 1400 ksi | 1 mm/min; ISO 527 |
| 9.69 GPa | 1410 ksi | 5 mm/min; ASTM D 638 | |
| Flexural Yield Strength | 203 MPa | 29400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
| 218 MPa | 31600 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 8.61 GPa | 1250 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
| 8.72 GPa | 1260 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 1.07 J/cm @Temperature 23.0 °C |
2.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
| Izod Impact, Unnotched | 8.54 J/cm @Temperature 23.0 °C |
16.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
| Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
| 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | 47.0 kJ/m² @Temperature 23.0 °C |
22.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
| 49.0 kJ/m² @Temperature -30.0 °C |
23.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U | |
| Charpy Impact Unnotched | 5.50 J/cm² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
| 5.50 J/cm² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU | |
| Charpy Impact, Notched | 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA | |
| Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 150 °C |
10.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
| 18.0 µm/m-°C @Temperature 23.0 - 150 °C |
10.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature -40.0 - 150 °C |
32.2 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
| 58.0 µm/m-°C @Temperature 23.0 - 150 °C |
32.2 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
| 191 °C @Thickness 3.20 mm |
376 °F @Thickness 0.126 in |
unannealed; ASTM D 648 | |
| 193 °C @Thickness 6.40 mm |
379 °F @Thickness 0.252 in |
unannealed; ASTM D 648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 169 °C | 336 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| 182 °C @Thickness 3.20 mm |
360 °F @Thickness 0.126 in |
unannealed; ASTM D 648 | |
| 185 °C @Thickness 6.40 mm |
365 °F @Thickness 0.252 in |
unannealed; ASTM D 648 | |
| Vicat Softening Point | 190 °C | 374 °F | Rate B/50; ISO 306 |
| 192 °C | 378 °F | Rate B/120; ISO 306 | |
| 193 °C | 379 °F | Rate B/50; ASTM D 1525 | |
| Flammability, UL94 | V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
UL 94 |
| 5VA @Thickness 3.00 mm |
5VA @Thickness 0.118 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.10e+16 ohm-cm | 1.10e+16 ohm-cm | IEC 60093 |
| Surface Resistance | 2.30e+16 ohm | 2.30e+16 ohm | ROA; IEC 60093 |
| Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
| Dissipation Factor | 0.0035 @Frequency 1000 Hz |
0.0035 @Frequency 1000 Hz |
IEC 60250 |
| 0.0037 @Frequency 50.0 - 60.0 Hz |
0.0037 @Frequency 50.0 - 60.0 Hz |
IEC 60250 | |
| 0.0096 @Frequency 1.00e+6 Hz |
0.0096 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 125 V | 125 V | IEC 60112 |
| >= 125 V | >= 125 V | IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | Passes | IEC 60695-10-2 |