Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics CHO-SHIELD® 576 Part B Coating Catalyst

Category Other Engineering Material , Catalyst/Initiator , Polymer , Adhesive
Manufacturer Parker Chomerics
Trade Name CHO-SHIELD®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SHIELD® 576 Part B Coating Catalyst.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity <= 1.00 g/cc
<= 1.00 g/cc
Volatiles 80 %
80 %
Solubility in Water 0.00 %
0.00 %
Insoluble
Thermal Properties Metric English Comments
Flash Point >= 7.22 °C
>= 45.0 °F
Descriptive Properties Value Comments
Butanol wt. % Max 10
Ethyl Benzene wt. % Max 5
Isopropanol wt. % max 5
Methyl isobutyl ketone wt. % 10 - 20
Physical Form Dark amber liquid
Polyamide Resin wt. % Max 30
Toluene wt. % Max 10 - 20
Vapor Density Heavier than air
Xylene wt. % 20 - 30
Users viewing this material also viewed the following: