Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Petroquimica Triunfo
Trade Name Trithene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding value to the printing and finish of the films. Its superior density in comparison to conventional LDPE allows the production of flasks with a greater stiffness and better resistance to the temperatures applied in sterilization processes in autoclaves. Because of its narrow molecular weight distribution and its branched structure, the Trithene® TX 3003 resin provides excellent processability with conventional extruders for LDPE, offers a low consumption of energy during processing, and allows the production of films and flasks with a good dimensional uniformity and excellent surface finish. This product complies with ASTM standard D1248-IIA5 and the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff. Applications: Shrink wrap films for the unitization of bottles of soft drinks, beer, and other beverages, vegetable oils, and hygiene and cleaning products. Bags with a high resistance for animal feed. Flexible flasks with a greater stiffness and better surface finish.Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.Information provided by Dax Resinas
Physical Properties Metric English Comments
Density 0.925 - 0.927 g/cc
0.0334 - 0.0335 lb/in³
ASTM D1505
Thickness 50.0 microns
1.97 mil
Melt Index of Compound 0.23 - 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.23 - 0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.0 MPa
2320 psi
ASTM D638
Tensile Strength, Yield 12.0 MPa
1740 psi
ASTM D638
Film Elongation at Break, MD 325 %
325 %
ASTM D882
Film Elongation at Break, TD 675 %
675 %
ASTM D882
Elongation at Break 620 %
620 %
ASTM D638
Secant Modulus, MD 0.125 GPa
18.1 ksi
5%; ASTM D882
Secant Modulus, TD 0.130 GPa
18.9 ksi
5%; ASTM D882
Coefficient of Friction, Dynamic 0.45
0.45
ASTM D1894
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 5.60 g/micron
142 g/mil
ASTM D1922
Dart Drop Test 200 g
0.441 lb
(method A); ASTM D1709
Film Tensile Strength at Break, MD 27.0 MPa
3920 psi
ASTM D882
Film Tensile Strength at Break, TD 24.0 MPa
3480 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 114 °C
237 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 7.5 %
7.5 %
ASTM D1003
Gloss 96 %
96 %
@ 60° Gardner; ASTM D2457
Processing Properties Metric English Comments
Processing Temperature 160 - 175 °C
320 - 347 °F
Plasticizing Zone
170 - 185 °C
338 - 365 °F
Mixture Zone
Feed Temperature 150 - 165 °C
302 - 329 °F
Adapter Temperature 180 - 195 °C
356 - 383 °F
Die Opening 0.0800 - 0.100 cm
0.0315 - 0.0394 in
Blow-up Ratio (BUR) 3.0
3.0
Recommended