Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Clearflex® RP 50 U Linear Medium Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Clearflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Clearflex® RP 50 U Linear Medium Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Clearflex RP 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RP 50 U show good mechanical properties and excellent surface aspect.Main Applications: Thanks to high processability, Clearflex RP 50 U is recommended for the production of items with difficult shapes, with inner smooth surface, toys and bas-reliefs.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.935 g/cc
0.935 g/cc
ISO 1183
Environmental Stress Crack Resistance >= 200 hour
>= 200 hour
ISO 22088
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ISO 868/A
Tensile Strength at Break 16.0 MPa
2320 psi
ISO 527
Tensile Strength, Yield 17.0 MPa
2470 psi
ISO 527
Elongation at Break >= 700 %
>= 700 %
ISO 527
Flexural Modulus 0.600 GPa
87.0 ksi
ISO 178
Dart Drop Total Energy 200 J/cm
0.375 ft-lb/mil
rotomolded sample; ISO 6603/2
Thermal Properties Metric English Comments
Melting Point 126 °C
259 °F
Internal method
Vicat Softening Point 113 °C

@Load 1.00 kg
235 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified