Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 9.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Polimeri Europa Europrene® SOL T 190 Styrene - Isoprene Block Copolymer
Europrene® SOL T 190 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and isoprene, where bound styrene content is 16% weight and diblock content is ..
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A Condition E; ASTM D1238
Network Polymers Kepital® F20-03
Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc.
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 260 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® MC8002 PC+ABS
AUTOMOTIVE. Low viscosity, high impact and ductility.
Melt Flow 9.0 - 16 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 - 16 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Polymer Resources PC-GP2-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Medium Flow
Polycarbonate, 5% PTFE, General Purpose, Medium Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp..
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Noble Polymers Regis™ 225104 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Melt Flow 9.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
cm³/10 min.
Ineos ABS Centrex® 814 ASA Blend  (discontinued **)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba..
Melt Flow 9.0 g/10 min
9.0 g/10 min
230/2.16 (typical); ASTM D1238
Fiberfil® J-69/10/E/UV High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled, UV Stabilized
Information provided by FIBERFIL Engineered Plastics
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
LG Chemical LUCEL HI515W POM+Rubber, High Impact
Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Kraton® D1160 E (SIS) Linear Triblock Copolymer
Description: Kraton D1160 E is a clear linear triblock copolymer based on styrene and isoprene with bound styrene of 18.5% mass. It is supplied from Europe in the physical form identified: D1160 ES ..
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Lucobit Lucofin® 1461 Polyolefin TPO Granules, Ice Blue
Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi..
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Lucobit Lucolit® 1321 Polyolefin TPO Granules, Blue
Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi..
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Lucobit Lucofin® 1455MB Polyolefin TPO Granules, Black
Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi..
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Lucobit Lucofin® 1459 Polyolefin TPO Granules, Azure Blue
Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi..
Melt Flow 9.0 g/10 min

@Load 6.60 kg,
Temperature 337 °C
9.0 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM 2210R PEI
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 400 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res..
Melt Flow 9.0 g/10 min
9.0 g/10 min
ASTM D1238
SPS Guang Zhou SAMATâ„¢ 168(f1) Flame-retarded Polypropylene
Characteristic: Good flame resistance, good chemical resistance, good mechanical propertiesApplications: X'mas decorative product, E/E applianceInformation Provided by SPS (Guang Zhou) Ltd.
Melt Flow 9.0 - 12.9 g/10 min
9.0 - 12.9 g/10 min
Shuman 502 Black Polypropylene Copolymer
Good impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer.
Melt Flow 9.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Styrolution Novodur® H801 ABS / PC
Novodur H801 is a high heat injection molding grade with high impact strength and reduced emission.Information provided by Styrolution
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Borealis Borstar® CB9600 HDPE for Extrusion Coating
Borstar CB9600 is the first bimodal high-density coating grade produced using the unique Borstar PE technology. The process controls the polymer `s molecular structure and is designed to produce bi..
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
A. Schulman POLYBATCH™ Metallic Grey 80330/2
DescriptionPOLYBATCH® Metallic Grey 80330/2 is a metallic grey color concentrate based in LDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH..
Melt Flow 9.0 - 14 g/10 min

@Load 2.16 kg,
Temperature 280 °C
9.0 - 14 g/10 min

@Load 4.76 lb,
Temperature 536 °F
Z-011A
Zeon Chemicals Zeonex® 330R Cyclo-Olefin Polymer
Zeonex®330R has a lower birefringence than other Zeonex® products. This grade can satisfy market demands in the optical area where low birefringence and high dimensional stability in precision opt..
Melt Flow 9.0 - 14 g/10 min

@Temperature 230 °C
9.0 - 14 g/10 min

@Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer
DescriptionPolyfort® FPP 2121UV-M-31 is a 30% black filled polypropylene homopolymer. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman...
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polyram RamTal PM1609 Acetal, Molybdenum Disulfide Filled
Molybdenum disulfide filled polyacetal for injection molding applications.Information provided by Polyram Ram On Ind.
Melt Flow 9.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238
Cossa Polimeri ESTADIENE 1020 HHT Acrylonitrile Butadiene Styrene
ABS with very high heat resistanceGood melt flow rate, good impact resistance, stiff, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Chevron Phillips K-Resin® KK38 Styrene-Butadiene Copolymer, Sheet Grade
Styrene-Butadiene CopolymerCustomer Benefits: KK38 is an improved extrusion grade SBC designed specifically for superior performance in blends with general purpose polystyrene. It is easily process..
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Extrusion, Black, Halogen Free
Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and..
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Extrusion, Natural, Halogen Free
Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and..
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
DuPont™ Appeel® 20D784 Ethylene Acrylate
Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature ..
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Azoty Tarnow™ TARNOFORM 300 POM
Basic, fast cycling injection molding grade suitable for many applications.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Melt Flow 9.0 g/10 min
9.0 g/10 min
Custom Resins Duratel™ MF9 Acetal Copolymer  (discontinued **)
Description: Duratel™ MF9 is a 9 melt flow, general purpose acetal copolymer. Information provided by Custom Resins.