| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergamid™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Bergamid™ A70 G15 HW TM-Z Polyamide 66 (Nylon 66).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 100 MPa @Temperature 23.0 °C |
14500 psi @Temperature 73.4 °F |
ISO 527-2 |
| Elongation at Break | 3.0 % @Temperature 23.0 °C |
3.0 % @Temperature 73.4 °F |
ISO 527-2 |
| Tensile Modulus | 4.80 GPa @Temperature 23.0 °C |
696 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179 | |
| Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| 1.10 J/cm² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 261 °C | 502 °F | ISO 3146 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Heat Stabilizer | |
| Hydrolysis Resistant | ||
| Impact Modifier | ||
| Features | General Purpose | |
| Filler / Reinforcement | Glass Fiber Reinforcement, 15% Filler by Weight | |
| Forms | Granules | |
| Generic Material | Nylon 66 | |
| Generic Name | Polyamide 66 (Nylon 66) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America |