| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Fittings 87322 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
| Spiral Flow | 78.7 cm | 31.0 in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 83 | 83 | ASTM D2240 |
| Tensile Strength, Yield | 45.5 MPa | 6600 psi | Type I, 51 mm/min; ASTM D638 |
| Elongation at Break | 110 % | 110 % | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.76 GPa | 400 ksi | Type I, 51 mm/min; ASTM D638 |
| Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
| Flexural Modulus | 2.90 GPa | 421 ksi | ASTM D790 |
| Izod Impact, Notched | 0.850 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
1.59 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
| 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
| 77.8 °C @Thickness 6.35 mm |
172 °F @Thickness 0.250 in |
Annealed; ASTM D648 | |
| Flammability, UL94 | V-0 | V-0 | UL 94 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 199 - 210 °C | 390 - 410 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Agency Ratings | NSF 14 | |
| NSF 61 | ||
| NSF Type II | ||
| Features | High Impact Resistance | |
| Medium Flow | ||
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Injection Molding | |
| PVC Cell Classification | 16354 | ASTM D1784 |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Construction Applications |