| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 62 | 62 | 15 sec; ASTM D2240 |
| 70 | 70 | ASTM D2240 | |
| Tensile Strength at Break | 11.7 MPa | 1700 psi | 510 mm/min; ASTM D638 |
| Tensile Strength | 3.65 MPa @Strain 100 % |
529 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| Elongation at Break | 450 % | 450 % | 510 mm/min; ASTM D638 |
| Compression Set | 18 % @Temperature 23.0 °C, Time 79200 sec |
18 % @Temperature 73.4 °F, Time 22.0 hour |
ASTM D395 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 179 - 182 °C | 354 - 360 °F | |
| 188 - 204 °C | 370 - 399 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Biocide | |
| Features | High Gloss | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Seals | |
| Weatherstripping |