| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible R312AE Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
| Volatiles | 0.90 % @Thickness 1.91 mm, Temperature 90.0 °C |
0.90 % @Thickness 0.0752 in, Temperature 194 °F |
Loss; Method A; ASTM D1203B |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 66 | 66 | 15 sec; ASTM D2240 |
| Tensile Strength at Break | 15.9 MPa | 2310 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 370 % | 370 % | Type IV, 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -37.2 °C | -35.0 °F | ASTM D746 |
| Oxygen Index | 28 % @Thickness 3.18 mm |
28 % @Thickness 0.125 in |
ASTM D2863 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 171 - 179 °C | 340 - 354 °F | |
| 188 - 199 °C | 370 - 390 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Biocide | |
| UV Stabilizer | ||
| Change in Mass | 0.9% | ASTM D543; 23°C, 120 hr, in Mineral Oil |
| 0.9% | ASTM D543; 23°C, 120 hr, in Vegetable Oil | |
| Features | Flame Retardant | |
| Good Chemical Resistance | ||
| Oil Resistant | ||
| UV Absorbing | ||
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Construction Applications | |
| Flooring |