| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
| Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 107 | 107 | ASTM D785 |
| Hardness, Shore D | 82 | 82 | ASTM D2240 |
| Tensile Strength, Yield | 51.0 MPa | 7400 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.55 GPa | 370 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
| Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
| Izod Impact, Notched | 0.800 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 17.8 °C @Thickness 3.18 mm |
64.0 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 81 % @Thickness 0.851 mm, Wavelength 400 nm |
81 % @Thickness 0.0335 in, Wavelength 400 nm |
Internal Method |
| 86 % @Thickness 0.851 mm, Wavelength 700 nm |
86 % @Thickness 0.0335 in, Wavelength 700 nm |
Internal Method |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 188 - 207 °C | 370 - 405 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Agency Ratings | FDA Food Contact, Unspecified Rating | |
| Appearance | Clear/Transparent | |
| Features | ESD Protection | |
| Food Contact Acceptable | ||
| High Gloss | ||
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Bottles | |
| Film | ||
| Packaging | ||
| Sheet |