Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Rigid Extrusion L0148 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF PolyOne Geon™ Vinyl Rigid Extrusion L0148 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
15 sec; ASTM D2240
Tensile Strength, Yield 43.1 MPa
6250 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.84 GPa
412 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 78.0 MPa
11300 psi
ASTM D790
Flexural Modulus 2.80 GPa
406 ksi
ASTM D790
Izod Impact, Notched 1.50 J/cm
<br>@Thickness 3.18 mm,<br> Temperature 23.0 °C
2.81 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
1.60 J/cm
<br>@Thickness 3.18 mm,<br> Temperature 23.0 °C
3.00 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
Dart Drop Total Energy 60.1 J/cm
<br>@Temperature 23.0 °C
0.113 ft-lb/mil
<br>@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
102 J/cm
<br>@Temperature 23.0 °C
0.191 ft-lb/mil
<br>@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 67.0 µm/m-°C
37.2 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C
<br>@Thickness 3.18 mm
162 °F
<br>@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 182 - 193 °C
360 - 379 °F
Descriptive Properties Value Comments
Agency Ratings ASTM E 84
Ease of Sizing Good
Features Low Smoke Emission
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Extrusion
PVC Cell Classification 13354
ASTM D1784
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Profiles