| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Wire & Cable EHB400A Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.47 g/cc | 1.47 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 90 | 90 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 17.4 MPa | 2520 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 280 % | 280 % | Type IV, 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 105 °C | 221 °F | UL Temperature Rating |
| Oxygen Index | 29 % <br>@Thickness 1.91 mm |
29 % <br>@Thickness 0.0752 in |
ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 3.20e+15 ohm-cm | 3.20e+15 ohm-cm | ASTM D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 174 - 182 °C | 345 - 360 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Lead Stabilizer | |
| Agency Ratings | CSA LAG (Low Acid Gas) | |
| Features | Flame Retardant | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| HCL Evolution | 16% | CSA C22.2 No. 0.3 |
| Processing Method | Extrusion Coating | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Retention of Tensile Elongation | 96% | 136°C, 1.91 mm; 168 hr, UL Standard |
| Retention of Tensile Strength | 100% | 136°C, 1.91 mm; 168 hr, UL Standard |
| Uses | Building Wire Insulation | |
| Wire & Cable Applications | ||
| Wire Types | THHN | |
| THW | ||
| THWN |