| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Wire & Cable W1202 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
| Deformation | 21 % @Temperature 121 °C, Time 3600 sec |
21 % @Temperature 250 °F, Time 1.00 hour |
500 g; UL 1581 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 52 | 52 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 22.4 MPa | 3250 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 290 % | 290 % | Type IV, 510 mm/min; ASTM D638 |
| Tensile Modulus | 0.0167 GPa | 2.42 ksi | Type IV, 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 105 °C | 221 °F | UL Temperature Rating |
| Brittleness Temperature | -19.0 °C | -2.20 °F | ASTM D746 |
| Flammability, UL94 | V-0 @Thickness 0.749 mm |
V-0 @Thickness 0.0295 in |
ALL; UL 94 |
| Oxygen Index | 31 % @Thickness 1.91 mm |
31 % @Thickness 0.0752 in |
ASTM D2863 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 191 - 196 °C | 376 - 385 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Lead Stabilizer | |
| Agency Ratings | UL QMFZ2 | |
| UL QMTT2 | ||
| Features | Flame Retardant | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion Coating | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Building Wire Insulation | |
| Wire & Cable Applications | ||
| Wire Types | THHN | |
| THW | ||
| THW-2 | ||
| THWN | ||
| TW |