Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Synprene® RT-3890MS Thermoplastic Elastomer - SBC  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® RT-3890MS Thermoplastic Elastomer - SBC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
0.900 g/cc
0.900 g/cc
ASTM D792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 33
33
10 Sec; ASTM D2240
33
33
10 Sec; ASTM D2240
Tensile Strength, Yield 9.65 MPa
1400 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
9.65 MPa
1400 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
9.31 MPa

@Strain 300 %
1350 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
9.31 MPa

@Strain 300 %
1350 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 300 %
300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
300 %
300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Rebound 30 %
30 %
Bayshore; ASTM D2632
Tear Strength 64.9 kN/m
370 pli
Die C (graves), 20 in/min; ASTM D624
64.9 kN/m
370 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 41 %
41 %
Method B, 73°F(23°C), 22 hrs; ASTM D395
41 %
41 %
Method B, 73°F(23°C), 22 hrs; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D746