Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.0090 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Multibase Multi-Pro® 4008 T Polypropylene
Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: ConnectorsElectrical/Electronic ApplicationsAppliancesInformation provided by Multibase
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
Across Flow; ISO 2577
Polykemi AB SCANMID 6 B32^ E F30 Nylon 6, Glass Fiber Reinforced, Modified
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm
0.0090 - 0.011 in/in
Across Flow; ISO 2577
Polykemi AB SCANMID 6 B32^ E Q30 Nylon 6, Glass Fiber Reinforced, Modified
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
RheTech Products HP534-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Natural
Applications: Door trim panelsCenter consolesSteering columnsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
Across Flow; ISO 2577
Polykemi AB SCANMID 6 B12^ QF2515 Nylon 6, Glass Fiber and Mineral Reinforced
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
Across Flow; ISO 2577
Polykemi AB SCANMID 6 B22^ E F30 Nylon 6, Glass Fiber Reinforced, Modified
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0090 - 0.018 cm/cm
0.0090 - 0.018 in/in
FRISETTA Test Method
Nilit FRIANYL A63 KV40 Nylon 6.6 for injection molding, 40% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.0090 - 0.015 cm/cm
0.0090 - 0.015 in/in
Lehmann & Voss LUVOCOM® 1105-8292 PEEK, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
Linear Mold Shrinkage 0.0090 - 0.018 cm/cm
0.0090 - 0.018 in/in
Lehmann & Voss LUVOCOM® 1850-7692/BK PBT, with glass spheres and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Linear Mold Shrinkage 0.0090 - 0.014 cm/cm
0.0090 - 0.014 in/in
Lehmann & Voss LUVOCOM® 80-7626 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Linear Mold Shrinkage 0.0090 - 0.014 cm/cm
0.0090 - 0.014 in/in
Lehmann & Voss LUVOCOM® 80-7653 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Antistatic.No change of electric potential at bearings in case of separation of charge caused b..
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
Injection molded; ASTM D955
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester
Introduction: IROGRAN A92E 4860 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A92E 4860 is part of the HUNTSMAN ..
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
LG Chemical LUPOL HF-3202D High Flow Polypropylene, 20% Mineral Fillers, High Impact
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
Tool, Montell
LyondellBasell Hifaxâ„¢ AB220GC/1 Thermoplastic Olefin Resin
Key Features: fractional melt flow, high modulus, UV-stabilized, extrusion grade thermoplastic olefin resin, high flexural modulus, high impact strength, good weatherability, good processabilityAppl..
Linear Mold Shrinkage 0.0090 - 0.014 cm/cm
<br>@Thickness 3.20 mm,<br> Time 259000 sec
0.0090 - 0.014 in/in
<br>@Thickness 0.126 in,<br> Time 72.0 hour
ASTM D955
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm
0.0090 - 0.011 in/in
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm
0.0090 - 0.011 in/in
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim..
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm
0.0090 - 0.011 in/in
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
Linear Mold Shrinkage 0.0090 - 0.012 cm/cm
0.0090 - 0.012 in/in
ASTM D955
A. Schulman POLYFLAM™ RPP 1174 Talc Filled, Homopolymer Polypropylene
DescriptionPolyflam® RPP 1174 is a high performance talc filled homopolymer polypropylene product with UL V0 flammability and 105°C temperature index at 0.81 mm. RPP 1174 is non-dripping and has ..
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm
0.0090 - 0.011 in/in
ASTM D955
Diamond Polymers DIAMALOY XNY-1012U Polycarbonate/Polyester Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
MD; ASTM D955
Aclo Accutech Polypropylene Homopolymer HP0334W20L1 Wollastonite Reinforced
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM Data; MD
BASF Ultramid® 8202C HS BK-102 PA6 (Conditioned)
Ultramid 8202C HS BK-102 is a heat stabilized, low viscosity, pigmented black, PA6, injection molding homopolymer possessing a modified crystalline structure for increased property performance and f..
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM Data; MD
BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Conditioned)
Ultramid 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced PA6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined wi..
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM Data; MD
BASF Ultramid® B50 01 PA6
Ultramid B50 01 is a high-viscosity, general-purpose extrusion PA6 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyam..
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm
0.0090 - 0.011 in/in
Across Flow; ISO 2577
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
PlastxWorld CEVIAN® A1700 PA/ABS Alloy, Conditioned
Property data is for samples at equilibrium moisture (2.0%)Information provided by PlastxWorld Inc.
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
Injection; ASTM D955
Plaslok 308 Black (INJ) Mineral/Flock Filled Phenolic Molding Compound &nbsp;(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 308 is a two-stage, mineral and flock..
Copyright © lookpolymers.com All Rights Reserved