| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer |
| Manufacturer | PolyOne Corporation |
| Trade Name | Trilliant™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Trilliant™ HC X HC5200-0025 RS Natural Polypropylene Copolymer (PP Copolymer).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 70 | 70 | ASTM D785 |
| Tensile Strength, Yield | 24.8 MPa | 3600 psi | Type I, 51 mm/min; ASTM D638 |
| Elongation at Break | 60 % | 60 % | Type I, 51 mm/min; ASTM D638 |
| Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
| Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
| Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Izod Impact, Unnotched | 8.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.2 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
| Gardner Impact | 9.26 J @Thickness 3.18 mm, Temperature -23.0 °C |
6.83 ft-lb @Thickness 0.125 in, Temperature -9.40 °F |
ASTM D3029 |
| Dart Drop Total Energy | 6.73 J/cm | 0.0126 ft-lb/mil | Energy to Maximum Load; ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 118 °C @Thickness 3.18 mm |
244 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Impact Modifier | |
| Appearance | Natural Color | |
| Features | Copolymer | |
| Impact Modified | ||
| Specialty Grade | ||
| Filler / Reinforcement | Talc Filler | |
| Forms | Pellets | |
| Generic Material | PP Copolymer | |
| Generic Name | Polypropylene Copolymer (PP Copolymer) | |
| Processing Method | Injection Molding | |
| Regional Availability | North America | |
| Uses | Consumer Applications | |
| Disposable Hospital Goods | ||
| Hospital Goods | ||
| Industrial Applications | ||
| Medical/Healthcare Applications |