| Category | Polymer , Thermoplastic , Polypropylene (PP) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Trilliant™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Trilliant™ HC X HC5200-0026 RS Natural Polypropylene, Unspecified (PP, Unspecified).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 92 | 92 | ASTM D785 |
| Tensile Strength, Yield | 33.8 MPa | 4900 psi | Type I, 51 mm/min; ASTM D638 |
| Elongation at Break | 45 % | 45 % | Type I, 51 mm/min; ASTM D638 |
| Flexural Strength | 50.5 MPa | 7320 psi | ASTM D790 |
| Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D790 |
| Izod Impact, Notched | 0.370 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.693 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
7.49 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 124 °C @Thickness 3.18 mm |
255 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Natural Color | |
| Features | Medium Flow | |
| Specialty Grade | ||
| Filler / Reinforcement | Talc Filler | |
| Forms | Pellets | |
| Generic Material | PP, Unspecified | |
| Generic Name | Polypropylene, Unspecified (PP, Unspecified) | |
| Processing Method | Injection Molding | |
| Regional Availability | North America | |
| Uses | Disposable Hospital Goods | |
| Hospital Goods | ||
| Medical Appliances | ||
| Medical/Healthcare Applications |