Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Versaflex™ OM 2262 Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name Versaflex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Versaflex™ OM 2262 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Versaflex™ OM 2262 is a performance overmolding grade with general FDA compliance. This product is designed for both insert and two-shot molding onto Eastman Tritan™ copolyester as well as ABS, PC, and PC/ABS substrates.Color concentrates with EVA or LDPE carrier are most suitable for coloring Versaflex™ OM 2262. Typical letdown ratios are 50:1 to 25:1 - loading levels should be as low as possible to minimize the effect on adhesion. A high color match consistency can be obtained by the use of precolored compounds available from GLS. Concentrates based on PVC should not be used. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or poypropylene (PP). Regrind levels up to 20% can be used with Versaflex™ OM 2262 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt temperature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Versaflex™ OM 2262 has good melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 5 - 8 minutes or longer. Injection Speed: 0.5 to 2.5 in/sec 1st Stage - Boost Pressure: 200 to 900 psi 2nd Stage - Hold Pressure: 20-40% of Boost Hold Time (Thick Part): 4 to 10 sec Hold Time (Thin Part): 1 to 4 secInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Viscosity 21300 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
21300 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
Maximum Moisture Content 0.10
0.10
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
10 sec; ASTM D2240
Tensile Strength at Break 8.82 MPa

@Temperature 23.0 °C
1280 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress 2.60 MPa

@Strain 100 %,
Temperature 23.0 °C
377 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 660 %

@Temperature 23.0 °C
660 %

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Processing Properties Metric English Comments
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
Middle Barrel Temperature 177 - 199 °C
351 - 390 °F
Front Barrel Temperature 182 - 204 °C
360 - 399 °F
Nozzle Temperature 193 - 216 °C
379 - 421 °F
Melt Temperature 193 - 216 °C
379 - 421 °F
Mold Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Drying Temperature 51.7 - 54.4 °C
125 - 130 °F
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Back Pressure 0.000 - 0.552 MPa
0.000 - 80.1 psi
Screw Speed 50 - 100 rpm
50 - 100 rpm
Descriptive Properties Value Comments
Agency Ratings FDA Unspecified Rating
Please contact GLS Thermoplastic Elastomers for a copy of the FDA compliance letter.
Appearance Natural Color
Features Good Adhesion
Good Colorability
Good Flow
Good Moldability
Pleasing Surface Appearance
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Suggested Max Regrind 20%
Uses Consumer Applications
Drink Lids
Household Goods
Kitchenware
Non-specific Food Applications
Overmolding
Soft Touch Applications
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved