| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.910 g/cc | 0.0329 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | With Flow; ISO 2577 |
| 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | Across Flow; ISO 2577 | |
| Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 40 @Time 15.0 sec |
40 @Time 0.00417 hour |
Polykemi |
| Tensile Strength at Break | <= 10.0 MPa | <= 1450 psi | ISO/R527 |
| Elongation at Yield | 9.0 % | 9.0 % | ISO/R527 |
| Flexural Modulus | 0.450 GPa @Temperature 23.0 °C |
65.3 ksi @Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 2.70 J/cm² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | 120°C/h; ISO 75/1 |
| Vicat Softening Point | 100 °C @Load 1.00 kg |
212 °F @Load 2.21 lb |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 200 - 230 °C | 392 - 446 °F | |
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure () | 20-40 | % of injection pressure |
| Injection Pressure | High | |
| Injection Speed () | High |