| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | Polykemi AB |
| Trade Name | SCANTEC |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polykemi AB SCANTEC PC S75R Polycarbonate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | With Flow; ISO 2577 |
| 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | Across Flow; ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | <= 60.0 MPa | <= 8700 psi | ISO/R527 |
| Elongation at Yield | 6.0 % | 6.0 % | ISO/R527 |
| Flexural Strength | <= 100 MPa | <= 14500 psi | ISO 178 |
| Flexural Modulus | 2.20 GPa @Temperature 23.0 °C |
319 ksi @Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 3.00 J/cm² @Temperature -20.0 °C |
14.3 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
| 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 140 °C | 284 °F | 120°C/h; ISO 75/1 |
| Deflection Temperature at 1.8 MPa (264 psi) | 130 °C | 266 °F | 120°C/h; ISO 75/1 |
| Vicat Softening Point | 140 °C @Load 5.001 kg |
284 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| 145 °C @Load 1.00 kg |
293 °F @Load 2.21 lb |
50°C/h; ISO 306 | |
| Flammability, UL94 | V-2 @Thickness 1.60 mm |
V-2 @Thickness 0.0630 in |
|
| Glow Wire Test | 850 °C @Thickness 2.00 mm |
1560 °F @Thickness 0.0787 in |
IEC 695-2-1 |