| Category | Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Blow Molding Grade , Linear Low Density Polyethylene (LLDPE), Injection Molded , Linear Low Density Polyethylene (LLDPE), Sheeting Grade |
| Manufacturer | Polyplastic Group |
| Trade Name | Armoflen® PO MF |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polyplastic Armoflen® PO MF 75-2 Linear Low Density Polyethylene, 75% Calcium Carbonate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.82 - 1.86 g/cc | 0.0658 - 0.0672 lb/in³ | ISO 1183 |
| Particle Size | 2.5 µm | 2.5 µm | |
| Melt Flow | 3.0 - 8.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
3.0 - 8.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Moisture Content | <= 0.10 % | <= 0.10 % |