Material Notes:
Nitrile Butadiene Rubber (NBR) 55-65 °IRHD. Medium acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet specification BS2751 BA60. Also meets obsolescent specification BS3222M.Applications: Excellent resistance to petroleum based oils and fuels. Excellent compression set, tear and abrasion resistance. Good water resistance, but poor against ozone and weather.
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
°IRHD; ASTM D1415
67
67
°IRHD, +5 change after 70 hours @ 70°C; ASTM D1415
Tensile Strength, Yield 8.50 MPa
1230 psi
-15% change after 70 hours @ 70°C; ASTM D412
10.0 MPa
1450 psi
ASTM D412
Elongation at Break 255 %
255 %
-15% change after 70 hours @ 70°C; ASTM D412
300 %
300 %
ASTM D412
Compression Set 15 %
15 %
24 hours @ 70°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-25.0 °C
-13.0 °F
Temperature at which stiffness does not exceed 70 Mpa
Flash Point >= 300 °C
>= 572 °F