| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Polyphenylene Ether/PPO |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics NORYL GTX870 PPE+PA6 (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
| Water Absorption | 0.50 % @Time 86400 sec |
0.50 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 117 MPa | 17000 psi | SABIC - Japan Method |
| 122 MPa | 17700 psi | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Break | 5.0 % | 5.0 % | Type I, 5 mm/min; ASTM D638 |
| 12 % | 12 % | SABIC - Japan Method | |
| Flexural Strength | 166 MPa | 24100 psi | ASTM D790 |
| Flexural Modulus | 5.68 GPa | 824 ksi | ASTM D790 |
| Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 40.0 - 60.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2 - 33.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
| Deflection Temperature at 1.8 MPa (264 psi) | 200 °C @Thickness 6.40 mm |
392 °F @Thickness 0.252 in |
unannealed; ASTM D648 |