Precision Polymer Engineering V75L Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V75L Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Special, steam-resistant Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK710, A1-10, B38, EF31, EO78, F15, Z1. Where Z1 = hardness 70-80.Applications: Compounded for improved resistance to acids, aqueous media and steam, as compared with other FKM elastomers. Excellent resistance to oils fuels and hydraulic fluids at high temperature.
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
°IRHD; ASTM D1415
85
85
°IRHD, +10 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 7.875 MPa
1142 psi
-25% change after 72 hours @ 250°C; ASTM D412
10.5 MPa
1520 psi
ASTM D412
Elongation at Break 142.5 %
142.5 %
-25% change after 72 hours @ 250°C; ASTM D412
190 %
190 %
ASTM D412
Compression Set 19 %
19 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -15.0 °C
5.00 °F
Flash Point >= 315 °C
>= 599 °F