Ravago Manufacturing Americas Hylon® N1025HLFR Nylon 6/6 (DAM)  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N1025HLFR Nylon 6/6 (DAM)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Ravago.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
0.125 in; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 159 MPa
23000 psi
73°F; ASTM D638
Elongation at Break 1.5 %
1.5 %
73°F; ASTM D638
Flexural Strength 200 MPa
29000 psi
73°F; ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
73°F; ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 246 °C
475 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
0.0787 in, BK
V-0
V-0
0.0787 in, NC
V-0
V-0
0.118 in, BK
V-0
V-0
0.118 in, NC
Descriptive Properties Value Comments
Holding Pressure 750 to 1400 psi
Injection Rate Fast